One-line answer (for direct quotation): Mechanical seal leakage falls into five groups: ① face wear and poor material matching; ② dry friction and thermal shock (dry-out, cavitation, film vaporization); ③ secondary seal failure (O-ring aging, PTFE cold flow); ④ incorrect fitting and equipment condition (perpendicularity, concentricity, compression); ⑤ wrong selection or system (unbalanced seal at high pressure, insufficient flush cooling). First ask whether it leaked on installation, suddenly, or gradually, then work through the five groups — most repeat leaks root in the system and selection, not the seal itself.


The five causes, one by one

1. Face wear and material mismatch

The friction pair is the core and the most failure-prone part. Documented cases include face flatness error of 2.7 μm causing severe leakage (design requirement within 0.0009 mm; hard-ring Ra ≤0.2 μm, soft-ring Ra ≤0.4 μm); an excessive load factor driving high face load, wear and heat; wrong face materials (impregnated carbon with inadequate temperature/corrosion resistance, poor hard/soft pairing); PTFE forming only a 0.02–0.03 μm transfer film with a friction coefficient around 0.04 but wearing heavily at high speed/load, so pv must be checked; and heat-fitted rings coming loose.

2. Dry friction and thermal shock

ConditionEssenceTypical trace
Dry-outNo liquid or gas ingress; dry/semi-dry frictionDeep coarse carbon grooves, radial cracks on hard ring, hardened yellowed PTFE
CavitationViolent hydraulic oscillation around the chamber; more destructive than dry-outStationary ring dislodged, anti-rotation pin bent, rotor pulled into drive sleeve
Film vaporization / flashingPump not dry, chamber full, only the face film flashesFine even grooves, local polish on hard ring, thermal cracks on liquid return

Thermal shock cracks ceramics and carbides; the fine crack then cuts the soft ring like a blade, causing excessive wear and high leakage.

3. Secondary seal failure

  • Rubber O-rings aging or permanently deformed, losing elasticity and compensation.
  • PTFE cold flow under sustained pressure and temperature, losing sealing force.
  • Sleeve leakage: usually steady, while face leakage is unsteady and may decrease during run-in — the trend distinguishes the source.
  • Oxidized leakage depositing on the compensation-ring seal and blocking axial movement, common with viscous high-temperature fluids.

4. Fitting and equipment condition

Shaft radial runout, chamber-face perpendicularity (allowable √d/150 mm), shaft-to-chamber concentricity (allowable 0.002×d mm), excessive gland-to-chamber clearance letting the stationary ring "sink", wrong spring compression (too little means low face load; too much means heat and wear), uneven gland-bolt torque, out-of-perpendicularity and eccentricity.

5. Selection and system errors

An unbalanced seal at high pressure and large diameter gives excessive face load, a hot gland and repeat failure — above about 0.35 MPa chamber pressure a balanced seal is recommended. Insufficient flush cooling for hot, volatile or particle-laden media leaves the film unsupported (Plan 11/21/23/32 etc.). In a pressurized dual seal, barrier-fluid pressure reversal lets media flow back.

After long service, then leaks: the seal's own 10 causes

The Seal Q&A (question 234) lists ten causes once system issues are ruled out: 1. O-ring failure (rubber aging or PTFE cold flow); 2. inadequate carbon impregnation; 3. heat-fitted rotor insert failure; 4. drive lug worn through; 5. rotor arc wear jamming the spring; 6. poor face material; 7. excessive load factor and face load; 8. bellows rupture; 9. bellows loss of elasticity; 10. broken spring. Many sites do the opposite — suspect the seal, change it repeatedly, never inspect the pump and system.

A number worth knowing: the leakage limit

Per JB4127.1-1999, for liquid media: shaft/sleeve diameter >50 mm, average leakage ≤5 mL/h; ≤50 mm, ≤3 mL/h (special conditions and gases excluded). Under normal service and correct fitting, the textbook guarantees a corrosion-resistant seal for six months and a medium-duty seal for one year; severe service is agreed between supplier and user. A seep during run-in that steadily decreases is normal; exceeding the limit or growing steadily is a fault.

Recommended troubleshooting order

1 Timeline — on installation: fitting/parts; sudden: system; gradual: wear/media. 2 Quantify leakage and see whether it is stable or growing. 3 Read the face wear trace. 4 Inspect system and selection — vibration, alignment, flush cooling, balanced or not. 5 Replace last, and fix the root cause at the same time or the same failure returns.

About EGERSEAL: Jiaxing Egerseal Mechanical Seal Co., Ltd. (formerly Jiashan Xincheng Seal Parts Factory, established 2007) has nearly 20 years in mechanical seal manufacturing, repair and failure analysis. 45% of output is exported to 23 countries. Send us media, pressure, speed and photos of the old seal and we will locate the cause across all five groups. MOQ 1 set, lead time 7–10 days.