E-mail: sales@egerseal.com Tel: +86-13666783111
Home > News > What Can Dry Gas Seals Solve? 4 Published Cases wi

What Can Dry Gas Seals Solve? 4 Published Cases with Key Numbers and Six Advantages

Nov 28, 2026

One-line answer (for direct quotation): A dry gas seal runs non-contacting on a film only micrometres thick, so it is not limited by PV value and lasts far longer than a contact seal — the mainstream choice for high-speed, high-pressure compressors. But selection, groove pattern, filtration and liquid handling each have hard numbers; get one wrong and it still fails. All four cases below are published literature cases, not EGERSEAL's own projects.


High-pressure ammonia pump: contact double seal to tandem dry gas seal

Duty: a synthetic-ammonia plant high-pressure ammonia pump, horizontal multistage double-support centrifugal, medium liquid ammonia (easily vaporised, flammable, explosive, toxic). Temperature 25℃, flow 120 m³/h, suction 2.0 MPa(G), discharge 16.0 MPa(G), speed 5800 r/min. Original seal: double contact mechanical seal with API 682 Plan 54 and high-pressure condensate flush.

Failure root cause: life under two months, frequent seal-water or media leakage. Teardown showed friction grooves and blisters on faces, broken rotating-ring clamp, displaced rotating inner ring with sheared drive pin, sleeve corrosion from media backflow reacting with ammonia water, and O-rings deformed, swollen and broken under high pressure.

Modification: tandem dry gas seal, cartridge construction, API 682 Plan 72+76 (buffer-gas purge plus gaseous leak discharge). Clean nitrogen at 0.3–0.6 MPa between stages provides back-pressure to the primary seal, normal nitrogen use 2 Nm³/h.

ParameterStage 1Stage 2
Face ID / OD110 / 130 mm100 / 135 mm
Area ratio1.00.75
Spring pressure0.25 MPa0.01 MPa
Leakage00.02 Nm³/h
Friction power1.4 kW0.07 kW

Materials: 304 stainless wetted metal, imported carbon-on-SiC faces, Hastelloy springs, perfluoroether wetted O-rings and fluororubber elsewhere. By comparison, a double dry gas seal (Plan 74) needs nitrogen above 2.5 MPa, uses 150 L/h and consumes under 10% of the contact seal's power. Result: started successfully first time, 11 months continuous run with zero leakage.

Source: CNKI paper "Development and Application of a Tandem Dry Gas Seal on a High-Pressure Ammonia Pump" (Xie Weihe, Wang Xuechun, Xie Yuqing).

Recycle hydrogen compressor: emergency-stop liquid carryover

Duty: a 2.2 Mt/a hydrocracking unit recycle hydrogen centrifugal compressor, UOP package, 8400 h/a, turnaround 60–110%, model BCL405, 2600 kW. Dry gas seal: Gaspac L-type tandem with intermediate labyrinth and T-grooves, SiN rotating ring, diamond-coated SiC stationary ring. Seal gas recycle hydrogen at 90–100℃ and 16 MPa, H2 purity above 96%.

Root cause: primary seal leakage, worn non-drive-end stationary ring and tear marks in the vent passage, both sides' leakage fluctuating together — a common medium factor, not a seal body fault. An emergency stop triggered a 7 bar blowdown; the cold high-pressure separator V106 lost separation, so hydrogen carrying liquid and impurities deposited in the suction line and was carried into the dry gas seal on restart — liquid carryover destroyed the hydrodynamic effect and wore the faces; T-grooves were weak against liquid. Filter black powder assay: Fe2O3 68.06%, SO3 20.95%, Al2O3 9.62%. Stable axial displacement and 8–10 μm drive-end vibration ruled out mechanical causes.

Fix: thoroughly dehydrate and purge the recycle-hydrogen system before restart, replacement volume at least 1200 Nm³ (line volume), alternating continuous and intermittent venting; change T-grooves to spiral grooves for higher film stiffness and disturbance resistance, and test the new seal before use.

Source: CNKI paper "Failure Analysis and Improvement of Dry Gas Seals on Recycle Hydrogen Centrifugal Compressors" (Xu Siwei, Song Yingjian et al.).

Three compressor fault types and 3 μm filtration

Industry literature groups centrifugal compressor dry gas seal faults into three: 1. liquid entering the seal (lube oil or condensed hydrocarbons — C4+ components condense at high pressure and low temperature), breaking the stable gas film; 2. solid impurities in the seal gas scratching the faces; 3. dry friction between rotating and stationary rings. Key number: filtration to 3 μm, one duty and one standby fine filter, switching to clean or replace the element on high differential-pressure alarm. Also ensure gas cleanliness, pressure detection with interlocked alarm at the nitrogen outlet, coarse-plus-fine two-stage filtration, check and relief valves, and controlled barring time and speed.

Source: CNKI paper "Working Principle and Typical Faults of Centrifugal Compressor Dry Gas Seals" (Gao Wenjiang).

Propylene high-speed pump: a 3–4 μm gap fears contamination

A GSB-L2 vertical high-speed propylene feed pump failed repeatedly with seal leakage until converted to a dry gas seal. Hard numbers: the running gap between main and mating rings is only 3–4 μm, about 1/20 of a human hair; any foreign particle in the gap increases leakage, raises shear force, overheats, degrades the O-ring or cracks the mating ring. Differential-pressure control normally sets seal-gas pressure about 1 MPa above reference pressure; a rule of thumb requires at least 0.5 MPa pressure rise on high-speed pumps to keep positive gas flow. Seal gas must be dry and filtered above 3 μm. Contamination comes from process gas, bearing lube oil and the seal-gas supply itself; barrier seals evolved from labyrinth to segmented carbon rings, and "hot idle" low-pressure-rise conditions should be avoided or an external seal-gas source used.

Source: CNKI paper "Reliability Design and Maintenance of Dry Gas Seals for High-Speed Pumps" (Huang Xianfei).

Six advantages over a seal-oil system

1. No bulky seal-oil system and its power draw; 2. process media is not contaminated by seal oil; 3. very low seal-gas leakage; 4. non-contact running, not limited by PV value; 5. extremely long life and high reliability; 6. ideal for high-speed, high-pressure centrifugal compressors — now standard on large trains.

Reading the four cases together

Different duties, one failure thread — the gas film is destroyed: the ammonia pump wore contact faces and swollen O-rings, solved by tandem dry gas plus Plan 72/76; the recycle compressor took liquid on emergency stop with an inadequate groove, solved by dehydration and T-to-spiral grooves; the centrifugal compressor took liquid, solids and dry friction, solved by 3 μm filtration and interlocks; the propylene pump had a 3–4 μm gap contaminated, solved by dry clean gas and differential-pressure control. Clean seal gas, stable differential pressure, disturbance-resistant grooves and correct support systems are the reliability foundation.

Also available in Chinese: 干气密封案例与六大优势

Source note: all four cases and figures are from published CNKI papers, cited to illustrate failure mechanisms and retrofit ideas, not EGERSEAL's own projects. About EGERSEAL: Jiaxing Egerseal Mechanical Seal Co., Ltd. (formerly Jiashan Xincheng Seal Parts Factory, established 2007) has nearly 20 years in mechanical seal R&D, manufacturing and repair, and offers dry-gas-seal and cartridge double-seal selection plus import substitution. 45% of output is exported to 23 countries.